Weft knitted mesh dyeing issues
Weft knitted mesh dyeing issues
Weft-knitted wire mesh is a special fabric commonly used in printing, filtration, screening and other fields. Since it needs to work under a certain tension, the quality of weaving and dyeing has an important impact on its function and lifespan.
1. Uneven dyeing: Uneven dyeing can cause the color of the woven wire mesh to be inconsistent. The reasons may be uneven dispersion of the dye, improper temperature, time and other conditions during the dyeing process.
2. Color spots: Color spots or uneven coating during the dyeing process can affect the appearance and performance of the woven wire mesh. The cause may be uneven dispersion of dye, poor penetration, etc.
3. Fading: If the dyed woven wire mesh fades, it will not only affect the appearance, but also affect its function. The cause may be improper temperature, time, and dye used during the dyeing process.